Litcius/Paper detail

Alternative Method for the Treatment of Hydrometallurgical Arsenic–Calcium Residues: The Immobilization of Arsenic as Scorodite

Xu Ma, Zidan Yuan, Guoqing Zhang, Jiaxi Zhang, Xin Wang, Shaofeng Wang, Yongfeng Jia

2020ACS Omega36 citationsDOIOpen Access PDF

Abstract

. The scorodite produced from both ACRs displayed good As stability at pH 4.95 (0.9 and 0.5 mg/L) via the toxicity characteristic leaching procedure (TCLP) method and at pH 3-7 (0.4-3.0 mg/L) via a 15 day short-term stability test.

Topics & Concepts

ArsenicGypsumSulfuric acidLeaching (pedology)Toxicity characteristic leaching procedureDissolutionChemistryLimeHazardous wasteNeutralizationNuclear chemistryMetallurgyWaste managementEnvironmental chemistryInorganic chemistryMaterials scienceEnvironmental scienceHeavy metalsOrganic chemistryImmunologyBiologySoil waterSoil scienceEngineeringAntibodyArsenic contamination and mitigationMine drainage and remediation techniquesFluoride Effects and Removal
Alternative Method for the Treatment of Hydrometallurgical Arsenic–Calcium Residues: The Immobilization of Arsenic as Scorodite | Litcius