Mechanism of Li nucleation at graphite anodes and mitigation strategies
Chao Peng, Arihant Bhandari, Jacek Dziedzic, John R. Owen, Chris‐Kriton Skylaris, Denis Kramer
Abstract
AIMD simulations show Li favours to nucleate near the zigzag than on the basal plane of graphite anodes due to the topological surface states near the edge. Chemical doping and potential control could be potential strategies to mitigate Li plating.
Topics & Concepts
NucleationGraphiteZigzagAnodeMaterials scienceBasal planeChemical physicsEnhanced Data Rates for GSM EvolutionDopingChemical engineeringNanotechnologyTopology (electrical circuits)Composite materialCrystallographyGeometryChemistryOptoelectronicsPhysical chemistryThermodynamicsComputer sciencePhysicsElectrodeEngineeringElectrical engineeringTelecommunicationsMathematicsAdvancements in Battery MaterialsAdvanced Battery Materials and TechnologiesExtraction and Separation Processes