Litcius/Paper detail

Comprehensive recovery of zinc, iron and copper from copper slag by co-roasting with SO2–O2

Da-wei Wang, Yanjie Liang, Lin Zhang, Cong Peng, Bing Peng

2022Journal of Materials Research and Technology20 citationsDOIOpen Access PDF

Abstract

In this study, a novel method to recover copper, zinc and iron from copper slag by SO2–O2 roasting-leaching-magnetic separation was proposed. The effect of roasting experiment conditions were roasting temperature of 900 °C, holding time of 120 min, and φSO2 (The volume fraction of SO2 in the mixed gas of SO2 and O2) of 90%. Under the leaching conditions of leaching temperature 80 °C, leaching time 1 h, liquid–solid ratio 14:1, and pH 7, 91.03% of copper and 85.04% of zinc can be recycled respectively. The iron in the leaching residue can be enriched and recovered by magnetic separation at a magnetic field strength of 3000 Gs for 40 min. The iron recovery rate is 85.88% with 53.86% of the iron grade in the concentrate.

Topics & Concepts

RoastingCopperLeaching (pedology)ZincMetallurgyMaterials scienceMagnetic separationZinc ferriteCopper slagEnvironmental scienceSoil scienceSoil waterMetal Extraction and BioleachingMetallurgical Processes and ThermodynamicsExtraction and Separation Processes
Comprehensive recovery of zinc, iron and copper from copper slag by co-roasting with SO2–O2 | Litcius