Few-layer and large flake size borophene: preparation with solvothermal-assisted liquid phase exfoliation
Feng Zhang, Liaona She, Congying Jia, Xuexia He, Qi Li, Jie Sun, Zhibin Lei, Zong‐Huai Liu
Abstract
-methyl pyrrolidone (NMP), and a relative small surface tension when using solvents is favorable for the exfoliation of bulk B. Four-layer thick borophene and an average lateral size of 5.05 μm can be obtained in acetone as the exfoliating solvent. The surface composition of the exfoliated few-layer borophene with large flake size hardly changes, while the chemical state of B changes to some extent because they are partly oxidized on the surface by contaminates before and after exfoliation. This acetone solvothermal-assisted liquid phase exfoliation technique can be used to prepare high quality borophene with large horizontal sizes, and it will provide the basis to study few-layer borophene with large sizes further.